Printing papers published in between 1950&quot;s and 1990&quot;s were treated with three methods such as distilled water washing, CaCO<sub>3</sub> solution washing and methyl cellulose solution coating for improving their conservational properties. Accelerated aging with 80℃ and 80% RH for 14 days was applied to the testing papers. Results showed that distilled water and CaCO<sub>3</sub> washing kept increased pH even after accelerated aging, but did not improve folding endurances for 1950&quot;s-60&quot;s papers. Methyl cellulose treatment did not increased pH of the old papers, but increased folding endurances remarkably for 1950&quot;s-60&quot;s papers even after accelerated aging. It suggests that methyl cellulose treatment after CaCO<sub>3</sub> washing should give improvements both in pH and folding endurance. #aged printing paper #paper conservation #accelerated aging #methyl cellulose #CaCOSUB3/SUB #pH #folding endurance

ABSTRACT
1. 서론
2. 재료 및 방법
3. 결과 및 고찰
4. 결론
인용문헌

DBpia에서 서비스 중인 논문에 한하여 피인용 수가 반영됩니다.
Insert title here
논문의 정보가 복사되었습니다.
붙여넣기 하세요.