In Comparison with W-C-N and SiO₂ Buffer Layer on Si Substrate for La0.67Sr0.33MnO₃ Layer

오류 신고하기

피인용 0

In Comparison with W-C-N and SiO₂ Buffer Layer on Si Substrate for La0.67Sr0.33MnO₃ Layer
검색

    초록·키워드

    Recently, there has been a great deal of interest in Perovskite magnetic oxide thin films for giant magnetoresistance (GMR) and colossal magnetoresistance (CMR) due to their physical properties and that offers potential for various devices such as magnetic field sensors and hard disk heads[1,2]. Though the GMR, CMR and TMR films have been successfully deposited on several single crystal substrates, these technology must be deposited by viable buffer layer on Si substrate for future semiconductor applications. So we suggest W-C-N buffer layer instead of SiO₂ buffer layer on Si substrate[3]. Polycrystalline thin films of La₀.₆₇ Sr₀.₃₃MnO₃ (La-Sr-MnO) were prepared by water-based sol-gel processed on nitrogen concentration of W-C-N and SiO₂ buffer layer. We studies application W-C-N diffusion barrier for La-Sr-MnO magnetic device at nitrogen gas flow 0 sccm to 2 sccm. The La-Sr-MnO thin films deposition by spinning process and the films annealed in air 3 hours at 80 0℃ in oxygen ambient. We studied the comparison with W-C-N and SiO₂ buffer layer effect on Si substrate for La-Sr-MnO Manganese oxide layer. We also examine the grain size, lattice constant, hysteresis loop, and other La-Sr-MnO properties which are presumably related with magnetic properties. Iron base amorphous films have been expected to be used in electronic signal conditioning and sensor application areas, since they show attractive capabilities based on their unique magnetoelastic properties, such as large magneto-mechanical coupling factors with both soft magnetic properties and large magnetostriction ... 전체 초록 보기

    최근 본 자료 전체보기

      UCI(KEPA) : I410-ECN-0101-2009-428-016709018