메뉴 건너뛰기
소속 기관 / 학교 인증
인증하면 논문, 학술자료 등을  무료로 열람할 수 있어요.
한국대학교, 누리자동차, 시립도서관 등 나의 기관을 확인해보세요
(국내 대학 90% 이상 구독 중)
고객센터 ENG
주제분류

추천
검색

논문 기본 정보

자료유형
학술저널
저자정보
(BITS Pilani) (BITS Pilani) (BITS Pilani) (BITS Pilani) (BITS Pilani) (BITS Pilani) (FGIET) (RMIT University) (BITS Pilani)
저널정보
대한금속·재료학회 Metals and Materials International Metals and Materials International Vol.30 No.3
발행연도
수록면
697 - 713 (17page)
DOI
10.1007/s12540-023-01519-2

이용수

표지
📌
연구주제
📖
연구배경
🔬
연구방법
이 논문의 연구방법이 궁금하신가요?
🏆
연구결과
이 논문의 연구결과가 궁금하신가요?
AI에게 요청하기
추천
검색

초록· 키워드

The MoS2nanoflakes can be a novel candidate as a solid lubricant in fabricating friction material for automotive brake-paddisc systems. In this paper, an investigation has been made to analyze the effect of MoS2nanoflakes on the mechanical andtribological behavior of the formulated copper-free low-metallic composite friction material. Three samples, namely S1,S2,and S3,have been fabricated containing different types of solid lubricant. Sample S1had a solid lubricant as graphite, whilesamples S2and S3had graphite mixed with solid lubricant MoS2with average flake sizes of 2 μm and 50 nm, respectively. Other components included steel, PAN, and aramid as reinforcing fibers; walnut powder, barium sulphate (BaSO4), andnitrile-butadiene rubber as fillers; phenolic resin as a binder; and FeO, Quartz, and MgO as abrasives. A pin-on-disc tribometertest (ASTM G-99) was conducted to carry out the wear test at a load of 60 N, sliding velocity of 2.09 m/s, and slidingdistance of 6283 m at room temperature. A scanning electron microscope was used to study the micro-structural evolutionof worn composite friction pin material. The results show that the nano-sized MoS2solid lubricant influences the structuralintegrity of the formulated composites, which governs the friction and wear behavior. The graphite and MoS2-based frictioncomposites S2and S3perform better than the conventional friction material (S1) containing graphite in terms of physical–mechanical, thermal, and tribological properties. The specific wear rate of the S1sample is the highest (2.72 × 10–5 mm3/Nm) followed by S2(1.84 × 10–5 mm3/Nm) and S3(0.98 × 10–5 mm3/Nm) respectively. The graphite and MoS2-based frictionspecimens S2and S3showed adequate coverage of friction plateaus, reducing wear and abrasion of the counter disc.