A U + 5 wt.% Al powder (written U-5Al), manufactured by centrifugal atomization, was used in this study to assess the feasibility of densifying UAl x + Al powder mixtures by Spark Plasma Sintering (SPS) and obtaining a final composition with a minimum content of UAl 2 that meets specifications of targets for 99 Mo production. The microstructure of the U-5Al powder was studied first and mainly consists of a mixture of UAl 2 primary dendrites and α -U phase. Three SPS conditions differing in terms of UAl x /Al volume ratio and dwell time at 800 K were tested. The sintered discs were characterized by X-ray diffraction, optical microscopy, scanning electron microscopy and energy dispersive spectroscopy. A very quick transformation of the U-5Al particles into a mixture of aluminides (UAl 2 + UAl 3 + UAl 4 , referred to UAl x ) was evidenced: only a few minutes were sufficient to transform the U-based particles into a mixture of aluminides containing about 80 wt.% of UAl 3 . According to these first tests, this new highly versatile manufacturing process could advantageously replace the conventional method of producing targets, subject to technical adjustments and parametric studies.
인공지능 문자 인식 모델을 통해 추출된 텍스트로, 일부 오타나 오류가 포함될 수 있으나 지속적으로 개선 중입니다.
오류를 발견하셨다면 해당 부분을 드래그한 후 ' 를 통해 신고해주세요.
오류를 발견하셨다면 해당 부분을 드래그한 후 ' 를 통해 신고해주세요.